| 1. | 12 Stages Chemical Pretreatment | 
                    
                      |  | Step 1 - Alkaline degreasing Step 2 - Tap water rinsing
 Step 3 - Tap water rinsing
 Step 4 - Etching & Desmutting
 Step 5 - Tap water rinsing
 Step 6 - Tap water rinsing
 Step 7 - Chromate conversion coating
 Step 8 - Deionized water rinsing
 Step 9 - Deionized water rinsing
 Step 10 - Deionized water rinsing
 Step 11 - Drying
 Step 12 - Quality inspection for chemical pretreatment
 | 
                    
                      | 2. | Dusts on coating surface are removed by air ionizing blowers. | 
                    
                      | 3. | Electrostatic spray applied acrylic coating with dry film thickness 25-30 microns. | 
                    
                      | 4. | Coated parts are thermal cured with metal surface temperature 170  - 200  for 10-15 minutes.
 | 
                    
                      | 5. | Quality inspection for coating layer. |